Method for manufacturing semiconductor device capable of improving etching rate ratio of insulator to refractory metal
Abstract
In a method for manufacturing a semiconductor device, an insulating layer is formed on a refractory metal layer, and a contact hole in the insulating layer by a dry etching process using an etching gas includes one of: a mixture gas of fluorocarbon and hydrogen; a mixture gas of hydrofluorocarbon and hydrogen; a gas of hydrofluorocarbon; and a fluorocarbon gas except for CF 4 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 15.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing a semiconductor device comprising the steps in sequence of: forming a refractory metal layer; forming an insulating layer on said refractory metal layer; and perforating a contact hole in said insulating layer by a dry etching process using an etching gas, said etching gas is a mixture gas of fluorocarbon and hydrogen comprising a flow rate ratio of hydrogen to fluorocarbon plus hydrogen in the mixture gas of about 10 to 50 percent.
- Claim 2Depends on #1
The method as set forth in claim 1, wherein said refractory metal layer is made of one of tungsten, tungsten alloy, molybdenum and molybdenum alloy.
- Claim 3Depends on #1
The method as set forth in claim 1, wherein said insulating layer is made of one of silicon oxide, silicon nitride and silicon oxide nitride.