Patents
US 6,004,501 A#683134 Most CitedExpiredUnited States (USPTO)Utility

Method of producing fast-fired cordierite bodies

59Forward Citations (#683134 Global)
2.2/yrCitation Velocity (#1720817 Global)
9.21Citation PageRank (#1215583 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cordierite body is produced by providing cordierite-forming raw materials as talc, calcined talc, MgO-forming component, magnesium aluminate spinel, SiO 2 -forming component, Al 2 O 3 -forming component, kaolin, calcined kaolin, and/or mullite, such that the quantity R is less than about 1.207. R is 0.253 (wt. % mullite powder) +0.278(wt. % SiO 2 powder) +0.00590(wt. % SiO 2 powder)(wt. % spinel powder) -0.0193(wt. % SiO 2 powder)(heating time at maximum temperature) -0.348(heating time at maximum temperature) -0.00237(mean heating rate from 25° C. to 1275° C.) +0.0736(wt. % alpha Al 2 O 3 powder)(mean particle size of alpha Al 2 O 3 powder) +0.0892(wt. % Al(OH) 3 powder)(mean particle size of Al(OH) 3 powder) -0.215(wt. % dispersible high surface area Al 2 O 3 -forming component) +2.392(log 10 (1+(wt. % MgO-forming component)(wt. % calcined kaolin))). The raw materials are intimately blended with effective amount of vehicle and forming aids to form a plastic mixture. A green body is formed, which is dried and heated from room temperature up to a maximum temperature of about 1360° C. to 1435° C. at an average heating rate of at least about 70° C. per hour and held at maximum temp

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 59.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a cordierite body, the method comprising: a) providing cordierite-forming raw materials selected from the group consisting of talc, calcined talc, MgO-forming component, magnesium aluminate spinel, SiO 2 -forming component, Al 2 O 3 -forming component, kaolin, calcined kaolin, mullite, and combinations thereof, chosen such that the quantity R is less than about 1.207, wherein R is defined as the solution to the following mathematical computation: 0.253 (wt. % mullite powder) +0.278(wt. % SiO 2 powder) +0.00590(wt. % SiO 2 powder)(wt. % spinel powder) -0.0193(wt

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗