Patents
US 6,001,918 A#9197852 Most CitedExpiredUnited States (USPTO)Utility

Silicone gel composition for use as a sealant and a filler for electrical and electronic components and a gel prepared from this composition

11Forward Citations (#9197852 Global)
0.4/yrCitation Velocity (#19496978 Global)
2.44Citation PageRank (#10570300 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A silicone gel composition comprising: (A) 100 parts by weight of an organopolysiloxane containing at least two alkenyl groups per molecule and having a viscosity of 0.01 to 100 Pa.s at 25° C.; (B) an organopolysiloxane containing at least two silicon-bonded hydrogen atoms per molecule and having a viscosity of 0.001 to 10 Pa.s at 25° C. in an amount sufficient to provide from 0.2 to 5 moles of silicon-bonded hydrogen atoms per one mole of alkenyl groups in component (A); (C) 0.01 to 15 parts by weight of a silica powder having a specific surface area of at least 50 m 2 /g; (D) 0.0001 to 1.0 part by weight of a diamine compound represented by the following general formula: R 1 2 N--R 2 --NR 1 2 wherein each R 1 is independently a hydrogen atom or an alkyl group having 1 to 4 carbon atoms, and R 2 is an alkylene group having 2 to 4 carbon atoms; and (E) a hydrosilylation catalyst in a catalytic quantity; wherein the weight ratio of component (D) to component (C) in said gel composition is from 0.0005 to 0.05; and the silicone gel composition cures to form a silicone gel having a loss elastic modulus at 25° C. and at a shear frequency of 0.1 Hz of from 1.0×10 2 to 1.0×10 4 Pa, and a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A silicone gel composition, comprising: (A) 100 parts by weight of an organopolysiloxane containing at least two alkenyl groups per molecule and having a viscosity of 0.01 to 100 Pa.s at 25° C.; (B) an organopolysiloxane containing at least two silicon-bonded hydrogen atoms per molecule and having a viscosity of 0.001 to 10 Pa.s at 25° C. in an amount sufficient to provide from 0.2 to 5 moles of silicon-bonded hydrogen atoms per one mole of alkenyl groups in component (A); (C) 0.01 to 15 parts by weight of a silica powder having a specific surface area of at least 50 m 2 /g; (D) 0.0001

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗