Abstract

A semi-rigid asphalt concrete that can be produced under ambient temperature by applying traditional cement concrete production method. A high temperature heating and great pressure rolling that are necessary for producing asphalt concrete in conventional skills are never being constraints while producing the semi-rigid asphalt concrete. The method of producing the semi-rigid asphalt concrete generates less air pollution than the traditional method for producing hot mix asphalt concrete. The semi-rigid asphalt concrete consists of cationic emulsified asphalt, type-I cement, F-type superplasticizer, Na-Carboxymethyl Cellulose (Na-CMC), calcium chloride(CaCl 2 ), stone dust, and III d, IV b, or VII a gradation aggregates. By applying the procedure of producing cement concrete, the semi-rigid asphalt concrete is completely produced after mixing, placing, and curing. The cationic emulsified asphalt and the F-type superplasticizer are first mixed to generate a mixture, and then pour the prepared CaCl 2 and Na-CMC solution for continuous mixing. After the mixture is mixing evenly, the cement, stone dust, fine aggregate, and coarse aggregate are sequentially pouring to the mixture for mix

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 29.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing semi-rigid asphalt concrete which comprises cement comprising the steps of: pouring cationic emulsified asphalt, whose weight is in the range of from 0.9 to 1.1 times said cement, into a mixing device; pouring superplasticizer, whose weight is about 0.03 times said cement, into said mixing device; pouring Na-Carboxymethyl Cellulose (Na-CMC), whose weight is in the range of from 0.09 to 0.11 times said cement, into said mixing device; pouring calcium chloride (CaCl 2 ), whose weight is about 0.01 times said cement, into said mixing device; adding said cement and s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 29 total)

PatentTitleYearCitations
CN 109,095,828 BAsphalt concrete and production process thereof20210
CN 103,572,683 ARubber asphalt mixture aggregate gradation optimizing method—7
CN 104,098,293 BA kind of multifactor multilevel visual analysis method that configures high-performance modified emulsified asphalt20160
US 2007173580 A1Inorganic-organic polymer nanocomposite and methods for making and using—3
US 7,455,476 B2Method of reconstructing a bituminous-surfaced pavement20081
CN 107,265,926 AInspire confidence in basalt fibre water-permeating pitch mixed material in one kind incorporation North America—4
CN 100,441,775 CMethod of upgrading gravel and/or dirt roads and a composite road resulting therefrom20080
CN 109,095,828 AA kind of bituminous concrete and its production technology—8
US 7,250,460 B1Inorganic-organic polymer nanocomposite and methods for making and using20074
CN 109,231,894 BAsphalt mixture for roads and preparation method thereof20210
CN 112,358,261 AIn-situ cold-recycling foamed asphalt mixture and cold-recycling pavement construction method—5
CN 109,231,894 AA kind of road asphalt mixture and preparation method thereof—16
CN 109,968,782 AA kind of modified pitch is coated material and preparation method thereof and mineral pellet modified asphalt waterproof coiled material and preparation method thereof—13
CN 111,499,324 ALow-toxicity phosphogypsum cemented macadam material and application thereof in road base course—8
CN 108,708,244 BHighway pavement base without cracks and preparation method thereof20230