Patents
US 5,986,008 A#7803567 Most CitedExpiredUnited States (USPTO)Utility

Propylene polymer composition and thermoformed object

13Forward Citations (#7803567 Global)
0.5/yrCitation Velocity (#17431498 Global)
1.90Citation PageRank (#15753122 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention is to provide a propylene polymer composition capable of producing heat molded products having excellent balance between rigidity and impact resistance and to provide heat molded products produced from the composition, such as films and pipes. The propylene polymer composition comprises 10 to 90% by weight of a propylene polymer (A) and 90 to 10% by weight of a propylene polymer (B). The propylene polymer (A) has MFR A (measured at 230° C. under a load of 2.16 kg) of 0.001 to 8 g/10 min, Tm (measured by a differential scanning calorimeter) of 95 to 145° C. and a density (d A ) of 885 to 905 kg/M 3 , and in this polymer, the content of constituent units derived from an α-olefin of 4 to 20 carbon atoms is in the range of 1.5 to 11% by mol. The propylene polymer (B) has MFR B (measured at 230° C. under a load of 2.16 kg) of 0.1 to 600 g/10 min, Tm (measured by a differential scanning calorimeter) of 145 to 170° C., a density (d B ) of 905 to 916 kg/m 3 , and in this polymer, the content of constituent units derived from an (α-olefin of 4 to 20 carbon atoms is in the range of 0 to 2% by mol. The MFR A and the MFR B satisfy the relation 0.1≦log (MFR B /MFR A )≦6.1,

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A propylene polymer composition comprising: (A) a propylene polymer in an amount of 10 to 90% by weight, said polymer having the following properties: (1) the melt flow rate, as measured at 230° C. under a load of 2.16 kg, is in the range of 0.001 to 8 g/10 min, (2) the temperature at the maximum peak position of an endothermic curve of said polymer measured by a differential scanning calorimeter is in the range of 95 to 145° C., (3) the density is in the range of 885 to 905 kg/m 3 , and (4) the content of constituent units derived from an α-olefin of 4 to 20 carbon atoms is in the range

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗