Abstract

A propylenic resin which is a homopolymer of propylene or a copolymer of propylene, has (i) intrinsic viscosity [ eta ] measured in decaline at the temperature of 135 DEG C. in the range of 0.5 to 10 deciliter/g and (ii) content of insoluble fraction in boiling n-heptane (W) in the range of 10 to 99 weight % and shows (iii) relation between relaxation time of rubber component measured by pulse NMR at the temperature of 30 DEG C. [T2HR(30): mu s], relaxation time of rubber component measured by pulse NMR at the temperature of 80 DEG C. [T2HR(80): mu s] and the content of insoluble fraction in boiling n-heptane (W) satisfying the following equations:T2HR(80)</=670-2.2xWT2HR(80)/T2HR(30)</=8.8+0.086xWand a propylenic resin composition comprising (A) 10 to 95 weight % of the propylenic resin, particularly a propylenic resin which is at least one kind selected from a homopolymer of propylene and copolymers of propylene containing 4 mol % or less of other olefinic units, and (B) 90 to 5 weight % of a propylenic random copolymer having intrinsic viscosity [ eta ] measured in decaline at the temperature of 135 DEG C. in the range of 0.5 to 10 deciliter/g and containing 10 to 80 mol %

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A propylenic resin composition comprising (A) 10 to 95 weight % of at least one kind selected from the group consisting of a homopolymer of propylene and copolymers of propylene containing 4 mol % or less of other olefinic units having (i) intrinsic viscosity [η] measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and (ii) content of insoluble fraction in boiling n-heptane (W) in the range of 10 to 99 weight % and showing (iii) relation between relaxation time of rubber component measured by pulse NMR at the temperature of 30° C. [T 2H R (30): μs], relax

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)