Patents
US 5,985,387 A#1616428 Most CitedExpiredUnited States (USPTO)Utility

Thermo-shrinkable polyester film

37Forward Citations (#1616428 Global)
1.4/yrCitation Velocity (#4107229 Global)
4.31Citation PageRank (#4220771 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In a thermo-shrinkable polyester film, the thermal shrinkage ratio in a main shrinking direction is about 20% or more after being treated in water of about 70° C. for about seconds, about 35 to about 55% after treated in water of about 75° C. for about 5 seconds, and about 50 to about 60% after being treated in water of about 80° C. for about 5 seconds. After the film is shrunk by about 5% by treatment in water of about 75° C. for about 10 seconds, the probability of the elongation at rupture of the film in the direction perpendicular to the main shrinking direction being about 20% or less, is about 10% or less. The ratio of τ 1 /τ 2 is about 0.05 to about 0.45, where τ 2 is the stress of shrinkage in a main shrinking direction of the film at about 90° C., and τ 1 is the stress of shrinkage in a direction perpendicular to the main shrinking direction of the film at about 90° C. The sealing strength of the film is about 1.2 kg/15 mm of width or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 37.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A thermo-shrinkable polyester film, wherein: the thermal shrinkage ratio in a main shrinking direction is about 20% or more after being treated in water of about 70° C. for about 5 seconds, about 35 to about 55% after treated in water of about 75° C. for about 5 seconds, and about 50 to about 60% after being treated in water of about 80° C. for about 5 seconds, and after the film is shrunk by about 5% by treatment in water of about 75° C. for about 10 seconds, the probability of the elongation at rupture of the film in the direction perpendicular to the main shrinking direction being about 2

  2. Claim 2Depends on #1

    A thermo-shrinkable polyester film according to claim 1, having a thickness of dispersion of about 6% or less.

  3. Claim 3Depends on #1

    A thermo-shrinkable polyester film according to claim 1, comprising a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗