US 5,963,840 A#520785 Most CitedExpiredUnited States (USPTO)Utility

Methods for depositing premetal dielectric layer at sub-atmospheric and high temperature conditions

68Forward Citations (#520785 Global)
2.5/yrCitation Velocity (#1280444 Global)
8.55Citation PageRank (#1376349 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides systems, methods and apparatus for high temperature (at least about 500-800° C.) processing of semiconductor wafers. The systems, methods and apparatus of the present invention allow multiple process steps to be performed in situ in the same chamber to reduce total processing time and to ensure high quality processing for high aspect ratio devices. Performing multiple process steps in the same chamber also increases the control of the process parameters and reduces device damage. In particular, the present invention can provide high temperature deposition, heating and efficient cleaning for forming dielectric films having thickness uniformity, good gap fill capability, high density, low moisture, and other desired characteristics.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 68.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for depositing an insulating layer on a substrate on a heater in a chamber, said process comprising the steps of: heating said heater to a temperature of at least about 500° C. and below a reflow temperature of a phosphosilicate glass (PSG) film to be deposited in said chamber; pressurizing said chamber to a pressure of between about 10 to about 760 torr; and introducing silicon, oxygen, and phosphorus into said chamber to deposit said phosphosilicate glass (PSG) film on said substrate on said heater at said temperature.

  2. Claim 2Depends on #1

    The process of claim 1 wherein said temperature is at least about 600° C.

  3. Claim 3Depends on #1

    The process of claim 1 wherein said temperature is at least about 650° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Part 2b-Deposited Dielectrics for VLSI", Semiconductor International, Werner Kern, RCA Laboratories, David Sarnoff Research Center, Princeton, NJ, pp. 122-129, (Jul. 1985).
  • A.C. Adams et al., "The Deposition of Silicon Dioxide Films at Reduced Pressure", J. Electrochem. Soc., vol. 126, No. 6, pp. 1042-1046, (1979).
  • A.C. Adams et al., The Deposition of Silicon Dioxide Films at Reduced Pressure , J. Electrochem. Soc. , vol. 126, No. 6, pp. 1042 1046, (1979).
  • F.S. Becker et al., "Process and Film Characterization of Low Pressure Tetraethylorthosilicate-Borophosphosilicate Glass", J. Vac. Sci. Technol. B4(3), pp. 732-744, (May/Jun. 1986).
  • F.S. Becker et al., Process and Film Characterization of Low Pressure Tetraethylorthosilicate Borophosphosilicate Glass , J. Vac. Sci. Technol. B4 ( 3 ), pp. 732 744, (May/Jun. 1986).