Patents
US 5,963,773 A#3411438 Most CitedExpiredUnited States (USPTO)Utility

Tungsten skeleton structure fabrication method employed in application of copper infiltration and tungsten-copper composite material fabrication method thereof

23Forward Citations (#3411438 Global)
0.8/yrCitation Velocity (#8559092 Global)
4.25Citation PageRank (#4315936 Global)
7Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A tungsten skeleton structure fabrication method employed in an application of a copper infiltration and tungsten-copper composite fabrication method includes the steps of forming a source powder by coating the tungsten powder surface having a purity of 99.9 weight percent and 2˜5 μm in size, with nickel by less than 0.06 weight percent (600 ppm), forming an injection molded admixture by admixing a source powder and a polymer binder, carrying out a powder injection molded with regard to the admixture, and obtaining a tungsten skeleton structure by removing the polymer binder from the resultant injection molded body. The method prevents the molded body from being unevenly shrunken during a liquid phase sintering for thereby decreasing its production cost.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 23.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A tungsten skeleton structure fabrication method, comprising the steps of: forming a source powder by coating a tungsten powder surface having a purity of 99.9 weight percent and 2˜5 μm in size, with nickel by less than 0.06 weight percent (600 ppm); forming an admixture by admixing the source powder and a polymer binder; carrying out a powder injection molding with regard to the admixture; and obtaining a tungsten skeleton structure by removing the polymer binder from the resultant injection molded body.

  2. Claim 2Independent Claim

    A method for fabricating tungsten-copper composite comprising the steps of: forming a source powder by coating a tungsten powder surface having a purity of 99.9 weight percent and 2˜5 μm in size, with nickel by less than 0.06 weight percent (600 ppm); forming an admixture by admixing a source powder and a polymer bind

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 23 total)

Non-Patent Literature (5)

  • B. Yang, R.M. German, "Study on Powder Injection Molding Ball Milled W-Cu Powders", ibid, 237-244.
  • B. Yang, R.M. German, Study on Powder Injection Molding Ball Milled W Cu Powders , ibid, 237 244.
  • J.L. Johnson, K.F. Hens, R.M. German, "W-Cu and Mo-Cu for Microelectronic Packaging Applications: Processing Fundamentals", Tungsten and Refractory Metals-1994, Proceedings, Ed.A.Bose and R.J. Dowding, MPIF, Princeton, NJ. 245-252, 1994.
  • J.L. Johnson, K.F. Hens, R.M. German, W Cu and Mo Cu for Microelectronic Packaging Applications: Processing Fundamentals , Tungsten and Refractory Metals 1994, Proceedings, Ed.A.Bose and R.J. Dowding, MPIF, Princeton, NJ. 245 252, 1994.
  • J.L. Johnson, R.M. German, "Phase Equilibria Effects on the Enhanced Liquid Phase Sintering of Tungsten-Copper", Metallurgical Transactions A. vol. 24A, 2369-2377, 1993.