Reduced bird's beak field oxidation process using nitrogen implanted into active region
Abstract
A method of forming a self-aligned field oxide isolation structure without using silicon nitride. The method comprises forming a dielectric on an upper surface of a semiconductor substrate. The upper surface of the semiconductor substrate comprises an active region and an isolation region laterally adjacent to each other. A photoresist layer is patterned on top of the implant dielectric to expose regions of the implant dielectric over the active region. Nitrogen is then implanted into the active region through the implant dielectric. Nitrogen is preferably introduced into semiconductor substrate in an approximate atomic concentration of 0.5 to 2.0 percent. After the nitrogen has been implanted into a semiconductor substrate, the photoresist layer is stripped and the implant dielectric is removed. The wafer is then thermally oxidized such that a field oxide having a first thickness is grown over the isolation region and a thin oxide having a second thickness is grown over the active region. The presence of the nitrogen within the semiconductor substrate retards the oxidation rate of the silicon in the active region such that the thickness of the thin oxide is substantially less than
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 49 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A semiconductor substrate comprising: an active region within a semiconductor substrate, wherein said active region contains approximately 0.5 to 2.0 percent nitrogen within a thickness less than 200 angstroms of a surface of said semiconductor substrate; and an isolation region within said semiconductor substrate, laterally adjacent to said active region, wherein said isolation region comprises a thermal oxide formed on said semiconductor substrate.
- Claim 2Depends on #1
The semiconductor substrate of claim 1 wherein said thermal oxide has a thickness of approximately 2000 to 8000 angstroms and further wherein said thermal oxide includes a sidewall, proximal to said active region, extending substantially perpendicularly from an upper surface of said semiconductor substrate.
- Claim 3Depends on #1
The semiconductor substrate of claim 1 wherein sa
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (49)
Non-Patent Literature (5)
- Abbas et al., "Improvement of the Gate-Region Integrity in FET Devices," IBM Technical Disclosure Bulletin, vol. 14, No. 11, Apr. 1972, pp. 3348-3350.
- Abbas et al., Improvement of the Gate Region Integrity in FET Devices, IBM Technical Disclosure Bulletin , vol. 14, No. 11, Apr. 1972, pp. 3348 3350.
- Ahn, J. et al., "High Quality Ultrathin gate Dielectrics Formation by Thermal Oxidation of Si in N20," J. Electrochem. Soc. V. 139, No. 9, Sep. 1991, pp. L39-41.
- Ahn, J. et al., High Quality Ultrathin gate Dielectrics Formation by Thermal Oxidation of Si in N20, J. Electrochem. Soc. V. 139, No. 9, Sep. 1991, pp. L39 41.
- Cheung, "Plasma Immersion Ion Implantation for ULSI Processing," Trends & Applications, 1991, pp. 811-820.