The present invention is directed to a process for the preparation of a solid magnesium halide supported metallocene catalyst having a transition metal selected from the group consisting of IIIB, IVB, VB and VIB of the periodic table, which comprises preparing a slurry of magnesium metal in an electron donor solvent; heating the slurry of magnesium metal to 0° C. to 50° C. for a period of 10 minutes to 4 hr.; adding a dihaloalkane compound to said slurry to obtain a homogeneous solution of a support (solution A); separately preparing a solution of a metallocene compound in the same electron donor solvent as solution A (solution B); heating the solution B to 0° C. to 50° C. for a period ranging between 10 minutes and 1 hr., adding solution B to solution A over a period ranging between 10 minutes to 2 hrs. while maintaining the temperature in the range of 0 to 50° C. to obtain a homogeneous solution; cooling the resultant homogeneous solution to room temperature under an inert atmosphere; pouring the reaction mixture into a liquid hydrocarbon medium in which all the components will be partly or completely insoluble to precipitate the solid catalyst; separating the solid catalyst prec

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of a solid magnesium halide supported metallocene catalyst having a transition metal selected from the group consisting of IIIB, IVB, VB and VIB of the periodic table, which comprises preparing a slurry of magnesium metal in an electron donor solvent; heating the slurry of magnesium metal to 0° C. to 50° C. for a period of 10 minutes to 4 hr.; adding a dihaloalkane compound to said slurry to obtain a homogeneous solution of a support (solution A); separately preparing a solution of a metallocene compound in the same electron donor solvent as solution A (solution B

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • European Patent Office database "esp@cenet", Abstract of JP 4275311, published Sep. 30, 1992, Idemitsu Petrochem Cp. Ltd.
  • European Patent Office database esp cenet , Abstract of JP 4275311, published Sep. 30, 1992, Idemitsu Petrochem Cp. Ltd.