Process for stainless steel pickling and passivation without using nitric acid
Abstract
Process for stainless steel pickling consisting in placing the material to be treated in a bath kept at a temperature ranging from 30° C. to 70° C. having the following initial composition: a) H 2 SO 4 150 g/l at least b) Fe 3+ 15 g/l " " c) HF 40 g/l " " d) H 2 O 2 (added with known stabilizers) 1-20 g/l e) emulsifiers, wetting agents, polishing agents, acid attack inhibitors; in the bath being fed continuously: an air flow equal at least to 3 m 3 /h per m 3 bath min. and a stabilized H 2 O 2 quantity adjusted to the bath redox potential to be kept at ≧250 mV.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 27.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Pickling process for chromium containing stainless steel comprising placing said chromium containing stainless steel in a pickling bath kept at a temperature ranging from 30° C. to 70° C. and wherein said pickling bath prior to placing said chromium containing stainless steel in said pickling bath comprises the following components: a) H 2 SO 4 in an amount of at least 150 g/l; b) Fe +3 ions in an amount of at least 15 g/l; c) HF in an amount of at least 40 g/l; d) stabilized H 2 O 2 , which develops 130 liters of O 2 /l, in an amount between 1 and 20 g/l; e) non-ionic surfactants
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗