Process for forming improved cobalt silicide layer on integrated circuit structure using two capping layers
Abstract
The formation of a cobalt silicide layer of uniform thickness over the source/drain regions and the polysilicon gate electrode of an MOS structure, which does not thin out adjacent the edges of the top surface of the polysilicon gate electrode, i.e., adjacent the oxide spacers, is achieved by first forming a titanium capping layer over a cobalt layer deposited over the MOS structure prior to formation of the cobalt silicide, and while excluding oxygen-bearing gases from the cobalt surface prior to the deposition of the titanium capping layer. Oxygen-bearing gases are then excluded from contact with the titanium capping layer prior to at least the initial annealing step to form cobalt silicide, by forming a protective titanium nitride layer over the titanium layer, either: (1) in the same chamber used to deposit the titanium layer, or (2) while still maintaining the titanium-coated semiconductor substrate in an oxygen-free atmosphere during transfer of the titanium-coated semiconductor substrate from the titanium deposition chamber to a separate titanium nitride deposition chamber. In either event, the titanium capping layer is deposited over the cobalt layer, and the protective tit
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 80.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for forming an MOS structure on a silicon substrate comprising cobalt silicide contacts formed over the source/drain regions of said MOS structure and over a polysilicon gate electrode of said MOS structure which comprises: a) forming a cobalt layer over said MOS structure; b) forming a titanium layer over said cobalt layer without exposing said cobalt layer to oxygen-bearing gases; c) forming a titanium nitride layer over said titanium layer without exposing said titanium layer to oxygen-bearing gases; d) thereafter annealing said MOS structure at a first temperature to form c
- Claim 2Depends on #1
The process of claim 1 including the additional step of removing unreacted cobalt, titani
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 80 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (5)
- Berti, Antonio C., et al., "A Manufacturable Process for the Formation of Self Aligned Cobalt Silicide in a Sub Micrometer CMOS Technology", 1992 Proceedings Ninth International VLSI Multilevel Interconnection Conference (VMIC), Jun. 9-10, 1992, Santa Clara, CA, pp. 267-273.
- Berti, Antonio C., et al., A Manufacturable Process for the Formation of Self Aligned Cobalt Silicide in a Sub Micrometer CMOS Technology , 1992 Proceedings Ninth International VLSI Multilevel Interconnection Conference ( VMIC ), Jun. 9 10, 1992, Santa Clara, CA, pp. 267 273.
- Wang, Q.F., et al., "New CoSi2 Salicide Technology for 0.1 μm Processes and Below", 1995 Symposium on VLSI Technology Digest of Technical Papers, pp. 17-18.
- Wang, Q.F., et al., New CoSi 2 Salicide Technology for 0.1 m Processes and Below , 1995 Symposium on VLSI Technology Digest of Technical Papers, pp. 17 18.
- Yamazaki, Tatsuya, et al., "21 psec Switching 0.1 μm-CMOS at Room Temperature Using High Performance Co Salicide Process", IEDM 93, pp. 6.7.1.-6.7.3, 1993.