Patents
US 5,882,979 A#1703916 Most CitedExpiredUnited States (USPTO)Utility

Method for forming controllable surface enhanced three dimensional objects

36Forward Citations (#1703916 Global)
1.3/yrCitation Velocity (#4218267 Global)
3.54Citation PageRank (#5803695 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An embodiment of the present invention develops a process for controlling the grain size of a Hemi-Spherical Grained (HSG) silicon film by the steps of: performing a controlled implant of impurities into an amorphous silicon film; providing silicon seeding sites onto the surface of the amorphous silicon film; heat treating the amorphous silicon film, impregnated with the impurities and its surface having silicon seeding sites thereon, to cause HSG formation The implanting of the impurities into the amorphous material is controlled to place the impurities at a desired depth to thereby control the grain size of the HSG silicon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 36.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for controlling Hemi-Spherical Grain (HSG) formation, said process comprising the steps of: performing a controlled implant of impurities into an amorphous silicon film; providing silicon seeding sites onto the surface of said amorphous silicon film; after said steps of performing a controlled implant and providing silicon seeding sites, heat treating said amorphous silicon film to cause said HSG formation; wherein said process steps are performed ex-situ.

  2. Claim 2Depends on #1

    The process as recited in claim 1, wherein the surface of said amorphous silicon film is cleaned prior to said step of heat treating.

  3. Claim 3Depends on #1

    The process as recited in claim 1, wherein said step of performing a controlled implant comprises implanting said impurities into said amorphous silicon film at a depth to thereby control the size of the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 36 total)

PatentTitleYearCitations
US 6,632,719 B1Capacitor structures with recessed hemispherical grain silicon20034
US 7,092,233 B2Capacitor electrode having an interface layer of different chemical composition formed on a bulk layer20064
US 2004091634 A1Passivated magneto-resistive bit structure and passivation method therefor—0
US 7,427,514 B2Passivated magneto-resistive bit structure and passivation method therefor20080
US 6,825,522 B1Capacitor electrode having an interface layer of different chemical composition formed on a bulk layer20044
US 6,211,010 B1Method of forming hemispherical grains on a surface comprising pre-cleaning the surface in-situ with plasma20017
US 6,566,222 B2Methods of forming recessed hemispherical grain silicon capacitor structures20039
US 2006007631 A1Capacitor electrode having an interface layer of different chemical composition formed on a bulk layer—1
US 2004264240 A1Protective layers for MRAM devices—21
US 7,432,152 B2Methods of forming HSG layers and devices20080
US 6,479,364 B2Method for forming a capacitor for semiconductor devices with diffusion barrier layer on both sides of dielectric layer200228
US 6,326,277 B1Methods of forming recessed hemispherical grain silicon capacitor structures200117
US 6,930,015 B2Diffusion-enhanced crystallization of amorphous materials to improve surface roughness200511
WO 0,131,692 A1Method for manufacturing a capacitor by forming a silicon eletrode having hemispherical silicon—2
US 2003153142 A1Selective deposition of undoped silicon film seeded in chlorine and hydride gas for a stacked capacitor—5