Method of making developer compositions with stable triboelectric charging properties
Abstract
A method of preparing a developer composition involves the steps of: (1) blending carrier particles with finely divided toner particles, wherein blending is carried out for a period of time sufficient to enable the toner particles to alter the tribocharging ability of the carrier particles and become embedded therein; (2) dividing the blend of toner particles and carrier particles into coarse particles and fine particles; and (3) blending the coarse particles with toner particles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preparing a developer composition comprising the steps of: (1) blending carrier particles with finely divided toner particles, wherein blending is carried out for a period of time sufficient to enable the toner particles to alter the tribocharging ability of the carrier particles and become embedded therein; (2) removing fine particles and debris by dividing the blend of toner particles and carrier particles into coarse particles and fine particles; and (3) blending the coarse particles with toner particles.
- Claim 2Depends on #1
A method according to claim 1, wherein the finely divided toner particles in step (1) have an average diameter ranging from about 2 to about 10 microns.
- Claim 3Depends on #1
A method according to claim 1, wherein the finely divided toner particles in step (1) have an average diameter ranging from about 3
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗