Composite powder and manufacturing thereof for forming fluoro resin surface coating
Abstract
The composite resin powder having particle diameter range capable of being applied by way of fluidization dipping or electrostatic spray coating for forming a fluoro resin surface coating which melts at a lower temperature. 3.0 to 20 parts by weight of EAA resin is added to 100 parts by volume of xylene (86 parts by weight), the mixture is heated at 120° to 125° C. with stirring to dissolve, simultaneously PTFE powder with a particle diameter of 5 to 50 μm is added in an amount of 5 to 25% by weight to that of said EAA resin, then the temperature of the mixture was cooled to a temperature of 40° C. or lower to generate particles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 17.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A composite powder for double coating having a particle diameter of 10 to 300 μm as a whole and containing 5 to 25% by weight of PTFE powder having a particle diameter of 5 to 50 μm in EAA resin.
- Claim 2Independent Claim
A method for manufacturing composite resin powder in which 3.0 to 20 parts by weight of EAA resin is added to 100 parts by volume of xylene (86 parts by weight), the mixture is heated at 120° to 125° C. with stirring to dissolve, simultaneously PTFE powder with a particle diameter of 5 to 50 μm is added in an amount of 5 to 25% by weight to that of said EAA resin, then the temperature of the mixture was cooled to a temperature of 40° C. or lower to generate particles followed by solid-liquid separation.