Patents
US 5,872,322 A#1272590 Most CitedExpiredUnited States (USPTO)Utility

Liquid phase sintered powder metal articles

42Forward Citations (#1272590 Global)
1.6/yrCitation Velocity (#3260153 Global)
7.74Citation PageRank (#1622716 Global)
39Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of making a structural iron-based article comprising: (a) blending a compressible base iron powder (max. particle size of 100 microns) a graphite powder to provide carbon in mixture, and a single master alloy powder (average particle size of 10 microns) meltable within the range of 900°-1200° C. (1690°-2220 °F.) to form a mixture, the master alloy powder being present in an amount of 1-5% by weight of the mixture and consisting of (i) hardenability enhancing alloying ingredients selected from Mn, Mo, Ni, Cr, Cu and Fe, with Fe being present only if Cr or Mo is selected and (ii) wetting agents selected from the group of B, Y, Si and rare earth misch metal, the master alloy being devoid of carbon and being proportioned to provide a desired amount of hardenability in the base powder; (b) compacting the mixture to a green density 7.1-7.4 g/cm 3 to form a green part (c) machining the green part to a desired configuration if necessary; (d) sintering the green part to achieve liquification of the master alloy to densify the part to 7.3-7.5 g/cm 3 without substantially varying the configuration of the green; and (e) cooling the sintered part at a controlled rate to form a desired

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 42.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of making a structural iron-based article comprising: (a) blending a compressible iron-based powder and 1-5% by weight of a master alloy powder meltable in the temperature range of 900°-1200° C. (1690°-2200° F.) to form a mixture having admixture graphite in the range of 0.1-0.8% by weight; (b) compacting said mixture to a green density of 7.1-7.4 g/cm 3 to form a green part; (c) machining the green part to a desired configuration if necessary; (d) sintering the green part to effect liquification of only the master alloy without oxidation to densify the green part to 7.3-7.5 g/

  2. Claim 2Depends on #1

    The method as in claim 1 in which said master alloy has at least three selected f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 42 total)