A nickel powder having a composite oxide layer comprising lanthanum and nickel and, optionally an oxide of chromium, on at least a part of the surface thereof. The nickel powder is produced by a process comprising the steps of: bringing a solution comprising at least one heat-decomposable nickel compound and at least one heat-decomposable lanthanum compound and, optionally, at least one heat-decomposable chromium compound, to fine droplets; and heating the droplets at a temperature above the decomposition temperatures of these compounds to prepare a nickel powder and, at the same time, to deposit a composite oxide layer comprising lanthanum and nickel and, when present, chromium oxide, in the vicinity of the surface of the nickel powder. The nickel powder is suitable for use in a conductor paste to be co-fired with unfired ceramic green sheets for a multilayer component or the like because the sintering initiation of the powder is effectively delayed to around the sintering initiation temperature of the ceramic green sheets, thereby preventing the problems caused due to excessive sintering.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 19.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A nickel powder having a composite oxide layer comprising lanthanum and nickel on at least a part of the surface thereof.

  2. Claim 2Depends on #1

    A process for preparing a nickel powder according to claim 1, comprising the steps of: bringing a solution comprising at least one heat-decomposable nickel compound and at least one heat-decomposable lanthanum compound to fine droplets; and heating the droplets at a temperature above the decomposition temperatures of the nickel compound and the lanthanum compound to prepare a nickel powder and, at the same time, deposit a composite oxide layer comprising lanthanum and nickel in the vicinity of the surface of the nickel powder.

  3. Claim 3Independent Claim

    A nickel powder having a composite oxide layer comprising lanthanum and nickel and an oxide of chromium on at least a part of the surface thereof.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 19 total)

Non-Patent Literature (2)

  • Chemical Abstracts, vol. III, No. 8, Aug. 21, 1989, Abstract No. 61062, Furukawa, Sanehiro et al: "Anodes for molten-carbonate fuel cells "Abstract of JP 01 107 456 A.
  • Chemical Abstracts, vol. III, No. 8, Aug. 21, 1989, Abstract No. 61062, Furukawa, Sanehiro et al: Anodes for molten carbonate fuel cells Abstract of JP 01 107 456 A.