Methods for forming moisture blocking layers
Abstract
A method for forming an insulating layer for a microelectronic device includes the steps of forming a conductive pattern on a surface of a microelectronic substrate, and forming a spin-on-glass layer on the surface of the microelectronic substrate covering the conductive pattern. The spin-on-glass layer is baked at a temperature in the range of 400° C. to 750° C., and a moisture blocking layer is formed on the baked spin-on-glass layer. By reducing moisture absorbed from the air into the spin-on-glass layer, a relatively low etch rate and a relatively low dielectric constant can be maintained for the spin-on-glass layer. Related structures are also discussed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for forming an insulating layer for a microelectronic device, said method comprising the steps of: forming a conductive pattern on a surface of a microelectronic substrate; forming a spin-on-glass layer on said surface of said microelectronic substrate covering said conductive pattern; baking said spin-on-glass layer at a temperature in the range of 400° C. to 750° C. forming a moisture blocking layer on said baked spin-on-glass layer; and annealing said spin-on-glass layer and said moisture blocking layer at a temperature in the range of approximately 700° C. to 750° C.
- Claim 2Depends on #1
A method according to claim 1 wherein said spin-on-glass layer is formed from a material chosen from the group consisting of silicate, siloxane, and hydrogen silsesquioxane.
- Claim 3Depends on #1
A method according to claim 1 wherein th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗