Process for the preparation of copolyester resin having low acetaldehyde content
Abstract
A copolyester resin having excellent physical properties and a low acetaldehyde content is produced by: polycondensing a mixture of terephthalic acid and isophthalic acid with a glycol in the presence of a phosphate compound to prepare a copolyester prepolymer having an intrinsic viscosity of more than 0.5 dl/g; subjecting the copolyester prepolymer to a first heat-treatment to obtain a pre-crystallized resin; and subjecting the pre-crystallized resin to a second heat-treatment, to obtain a copolyester resin having an intrinsic viscosity of 0.62 to 0.80 dl/g and a melting point of 190° to 240° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing a copolyester resin which comprises: (a) polycondensing a mixture of terephthalic acid and isophthalic acid with a glycol in the presence of a phosphate compound in an amount ranging from 0.005 to 0.2 parts by weight per 100 parts by weight of the copolyester resin to prepare a copolyester prepolymer having 5 to 30% by weight of the ethylene terephthalate repeating unit and 70 to 95% by weight of the ethylene isophthalate repeating unit and having an intrinsic viscosity of more than 0.5 dl/g as measured at 35° C. at a concentration of 0.3 g in 25 ml of o-chlorophenol;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (2)
- Encyclopedia of Polymer Science and Technology, vol. 11, pp. 62 128, (1988).
- Encyclopedia of Polymer Science and Technology, vol. 11, pp. 62-128, (1988).