Impact modifier combination for aromatic polyesters
Abstract
An improved toughened blend of an aromatic polyester with from 5 to 20 phr of an impact modifier, which impact modifier is a blend of (a) 80 to 85 weight percent of a core/shell impact modifier having a polybutadiene core and at least one shell formed from methyl methacrylate and styrene; and (b) 15 to 20 weight percent of a linear copolymer which contains from 50 to 85 parts of units derived from ethylene, from 5 to 40 parts of units derived from (meth)acrylic esters, and from 2 to 10 parts of a copolymerizable monomer containing an epoxy group. The toughened blend exhibits higher impact strength than would be calculated for the blend using a linear relationship based on values of notched Izod for two blends, each containing only one of the impact modifiers at an equal use level.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A toughened blend consisting essentially of an aromatic polyester with from 5 to 20 parts, per 100 parts of polyester, of an impact modifier, which impact modifier is a blend of (a) 80 to 85 weight percent of a core/shell impact modifier having (1) from 70 to 90 parts of a core of a rubber which is a homopolymer of butadiene or a copolymer of butadiene with up to about 30% of at least one copolymerized vinyl monomer; (2) at least one shell, which shell is a homopolymer of methyl methacrylate or a copolymer which contains a majority of units derived from either methyl methacrylate or styrene;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗