Patents
US 5,849,944 A#4593373 Most CitedExpiredUnited States (USPTO)Utility

Polyurethane elastomers having improved green strength and demold time, and polyoxyalkylene polyols suitable for their preparation

19Forward Citations (#4593373 Global)
0.7/yrCitation Velocity (#11176806 Global)
2.91Citation PageRank (#7964119 Global)
21Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Elastomers exhibiting decreased demold times and improved green strength are prepared by reacting a di- or polyisocyanate with a monodisperse polyoxypropylene diol having ultra-low unsaturation, and preferably prepared by the double metal cyanide.t-butyl alcohol catalyzed polymerization of propylene oxide. Further improved demold times and elevated elastomer physical properties are made possible by the use of multidisperse polyoxyalkylene polyether polyol blends having an overall unsaturation of less than 0.010 meq/g and a polydispersity of about 1.4 or greater.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An isocyanate-terminated prepolymer prepared by reacting an excess of a di- or polyisocyanate with a polyoxyalkylene polyol component having an average equivalent weight of from about 1000 Da to about 8000 Da, a polydispersity of 1.4 or greater, and an unsaturation of less than 0.010 meq/g, wherein said polyoxyalkylene polyol component comprises a polyoxypropylene polyol.

  2. Claim 2Depends on #1

    The prepolymer of claim 1 wherein said polyoxypropylene polyol component is a polyoxypropylene diol.

  3. Claim 3Depends on #2

    The prepolymer of claim 2 wherein said polyoxypropylene polyol component comprises a multidisperse blend of individual polyoxypropylene diols having different molecular weights.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,239,879 AThermoplastic polyurethane prepared from a poly-1,2-propylene ether glycol, a low molecular weight glycol and 2,4-tolylene diisocyanate198023
US 5,096,993 AThermoplastic polyurethane elastomers and polyurea elastomers made using low unsaturation level polyols prepared with double metal cyanide catalysts1992113
US 5,100,997 APreparation of elastomers using high molecular weight polyols or polyamines, said polyols prepared using a double metal cyanide complex catalyst199270
US 5,100,922 AMethod for producing a molded product of integral-skin polyurethane foam199240
US 5,106,874 AProcess for preparing elastomeric polyurethane or polyurethane-urea polymers, and polyurethanes so prepared199280
US 5,116,931 AThermoset polyurethane elastomers and polyurea elastomers made using high functionality, low unsaturation level polyols prepared with double metal cyanide catalysts199277
US 5,124,425 ACurable polyurethane composition excellent in flexibility199222
US 5,158,922 AProcess for preparing metal cyanide complex catalyst1992786
US 5,185,420 AThermoplastic polyurethane elastomers and polyurea elastomers made using low unsaturation level polyols prepared with double metal cyanide catalysts199396
US 5,300,535 AMethod for producing polyurethane flexible foam199435
US 5,340,902 ASpandex fibers made using low unsaturation polyols199448
US 5,470,813 ADouble metal cyanide complex catalysts1995758
US 5,482,908 AHighly active double metal cyanide catalysts1996454
US 5,496,496 AProcess for producing polyurethane elastomers199634
US 5,545,601 APolyether-containing double metal cyanide catalysts1996159

Non-Patent Literature (4)

  • C.P. Smith et al., "Thermoplastic Polyurethane Elastomers Made From High Molecular Weight Poly-L™ Polyols", Polyurethane World Congress 1991, Sep. 24-26, 1991, pp. 313-318.
  • C.P. Smith et al., Thermoplastic Polyurethane Elastomers Made From High Molecular Weight Poly L Polyols , Polyurethane World Congress 1991, Sep. 24 26, 1991, pp. 313 318.
  • J. W. Reisch et al., "Polyurethane Sealants and Cast Elastomers with Superior Physical Properties", 33rd Annual Polyurethane Marketing Conference Sep. 30,-Oct. 3, 1990, pp. 368-374.
  • J. W. Reisch et al., Polyurethane Sealants and Cast Elastomers with Superior Physical Properties , 33 rd Annual Polyurethane Marketing Conference Sep. 30, Oct. 3, 1990, pp. 368 374.