Patents
US 5,840,221 A#214913 Most CitedExpiredUnited States (USPTO)Utility

Process for making silicon carbide reinforced silicon carbide composite

105Forward Citations (#214913 Global)
3.8/yrCitation Velocity (#541433 Global)
12.65Citation PageRank (#718315 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process comprising the steps of: a) providing a fiber preform comprising a non-oxide ceramic fiber with at least one coating, the coating comprising a coating element selected from the group consisting of carbon, nitrogen, aluminum and titanium, and the fiber having a degradation temperature of between 1400 DEG C. and 1450 DEG C., b) impregnating the preform with a slurry comprising silicon carbide particles and between 0.1 wt % and 3 wt % added carbon c) providing a cover mix comprising: i) an alloy comprising a metallic infiltrant and the coating element, and ii) a resin, d) placing the cover mix on at least a portion of the surface of the porous silicon carbide body, e) heating the cover mix to a temperature between 1410 DEG C. and 1450 DEG C. to melt the alloy, and f) infiltrating the fiber preform with the melted alloy for a time period of between 15 minutes and 240 minutes, to produce a ceramic fiber reinforced ceramic composite.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 105.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process comprising the steps of: a) providing a fiber preform comprising a non-oxide ceramic fiber having at least one coating, comprising carbon, b) melting a matrix alloy comprising silicon and between 0.003 wt % and 10 wt % carbon dissolved therein to form a molten alloy, and c) infiltrating the fiber preform with the molten alloy.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the fiber preform comprises fibers comprising silicon carbide, and the dissolved carbon is present in the alloy in an amount corresponding to at least 50 % of its saturation level in the alloy when the alloy is heated to 1410° C.

  3. Claim 3Depends on #2

    The process of claim 2 wherein the fiber comprising silicon carbide has a degradation temperature of between 1410° C. and 1450° C. and the molten alloy has a temperature of between 1410° C. and 1450° C.

Technical Overview & Description