Hydroisomerization treatment process for feeds from the fisher-tropsch process
Abstract
The invention concerns a process for the hydroisomerisation treatment for feeds from the Fischer-Tropsch process. The catalyst is essentially constituted by 0.05% to 10% by weight of a precious metal and a silica (5-70%)/alumina support with a specific surface area of 100-500 m 2 /g. The catalyst has an average pore diameter of 1-12 nm, the pore volume of pores with diameters between the average diameter ±3 nm being more than 40% of the total pore volume. The dispersion of the precious metal is 20-100% and the distribution coefficient for the precious metal is greater than 0.1. The process is operated at 200°-450° C. at a partial pressure of hydrogen of 2 to 25 MPa with a VVH of 0.1-10 h -1 and a hydrogen/feed volume ratio of 100-2000.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 28.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the treatment of feeds from a Fischer-Tropsch process to obtain lubricating oils, characterised in that the feed having been optionally hydrotreated is hydroisomerised in a hydroisomerisation zone, the effluent obtained is fractionated to obtain an isomerised residue, said residue being dewaxed to obtain oil and a non oily fraction, and in that the hydroisomerisation zone is operated at a temperature of 200°-450° C., at aq pressure of 2-25 MPa, with an hourly space velocity of 0.1-10 h -1 and a hydrogen/hydrocarbon volume ratio of 100-2000, using a catalyst which consists essent
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗