Abstract

An efficient method of producing a microporous polyolefin membrane having improved tensile strength and pierce strength is provided, in which a solution having dissolved therein 5% by weight to 50% by weight of a polyolefin whose weight-average molecular weight is in the range of 5×10 5 to 2.5×10 6 and whose weight-average molecular weight to number-average molecular weight ratio is less than 10, is extruded and rapidly cooled to obtain a gel-like product which is then stretched and has remaining solvent removed therefrom.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 54.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a microporous polyolefin membrane comprising the steps of: preparing a polyolefin solution comprising 5% by weight to 35% by weight of a polyolefin having a weight-average molecular weight in the range of 5×10 5 to 2.5×10 6 , and having a weight-average molecular weight to number-average molecular weight ratio of less than 10, and 95% by weight to 50% by weight of solvent; extruding the solution through a die; cooling the extruded solution to form a gel-like product; stretching the gel-like product at a temperature no more than 10° C. above the melting point of the

  2. Claim 2Depends on #1

    The method of producing a microporous polyolefin membrane according to claim 1 wherein the pol