US 5,821,135 A#4812266 Most CitedExpiredUnited States (USPTO)Utility

Methods for and applications of making buried structures in semiconductor thin films

18Forward Citations (#4812266 Global)
0.6/yrCitation Velocity (#12265932 Global)
4.05Citation PageRank (#4667842 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A transparent substrate as formed on its front side a layer of amorphous silicon. A laser beam is used to irradiate through the backside of the transparent substrate in order to form buried nucleation sites within the amorphous silicon. The buried nucleation sites which are used as nucleation seeds are then used during a front side crystallization process in order to form large single silicon crystals over the substrate surface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a plurality of single silicon crystals over a substrate comprising: forming an amorphous silicon layer over a front-side of the substrate; forming a mask on a surface of the substrate; irradiating, with a laser beam, the amorphous silicon layer through the backside of the substrate at predetermined locations in accordance with a configuration of the mask, the irradiating providing poly-silicon nucleation sites near an interface region between the amorphous silicon layer and the frontside of the substrate at the predetermined locations; and crystallizing remaining sec

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 2015132927 A1Polysilicon manufacturing method that controls growth direction of polysilicon—1
CN 106,328,497 BLow-temperature polycrystalline silicon film, preparation method thereof and display device20200
US 2002197759 A1Amorphous silicon crystallization method—33
CN 106,033,707 APreparation method for polysilicon film—1
US 2002127830 A1Heating treatment device, heating treatment method and fabrication method of semiconductor device—2
US 2006134929 A1Heating treatment device, heating treatment method and fabrication method of semiconductor device—4
US 6,107,107 AAnalyzing an electronic circuit formed upon a frontside surface of a semiconductor substrate by detecting radiation exiting a backside surface coated with an antireflective material200056
US 6,193,796 B1Method of crystallizing silicon layer200144
US 6,423,585 B1Heating treatment device, heating treatment method and fabrication method of semiconductor device200221
US 7,410,850 B2Heating treatment device, heating treatment method and fabrication method of semiconductor device20080
CN 106,328,497 ALow-temperature polycrystalline silicon thin film and preparation method thereof and display device—4
US 6,337,233 B2Method of manufacturing a polycrystalline silicon layer200213
CN 103,594,355 BThe polysilicon manufacture method in polycrystalline silicon growth direction can be controlled20160
US 2005059222 A1Method of forming polycrystalline semiconductor layer and thin film transistor using the same—10
US 7,507,645 B2Method of forming polycrystalline semiconductor layer and thin film transistor using the same20091