Process for preparing polysiloxane microspheres with a narrow size distribution
Abstract
The present invention relates to a process to prepare polysiloxane microspheres with narrow size distribution having a particle size in the range of about 0.5 microns to about 10 microns. The first step involves combining, by weight, an optional anionic surfactant, a polymeric stabilizer, an hydroxide base, and water to form a first aqueous mixture to which is added a silane monomer to form a second aqueous mixture. The second aqueous mixture is then stirred at a temperature of from about 5° C. to about 90° C. for at least about 1 hours to form an aqueous dispersion comprising polysiloxane microspheres. The polysiloxane microspheres upon separation may be optionally washed with water and optionally dried at a temperature of up to about 300° C. The polysiloxane microspheres can be further optionally jet treated to yield polysiloxane microspheres with a narrow size distribution having a particle size in the range of about 0.5 microns to about 10 microns.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 32.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process to prepare polysiloxane microspheres with narrow size distribution having a particle size in the range of about 0.5 microns to about 10 microns comprising the steps of: (a) combining, by weight, about 0-100 parts of an anionic surfactant, from about 0.01 to about 100 parts of a polymeric stabilizer, from about 0.01 to about 100 parts of an hydroxide base, per about 500 to about 1000 parts of water to form a first aqueous mixture; (b) adding to said first aqueous mixture from about 5 to about 700 parts, by weight of the water from said first aqueous mixture, of a silane monomer to f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗