Method for producing lactide and apparatus used therefor

14Forward Citations (#6759103 Global)
0.5/yrCitation Velocity (#15191769 Global)
3.15Citation PageRank (#7010830 Global)
1Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The method for producing lactide includes the steps of (a) synthesizing lactide using lactic acid as a starting material; (b) discharging in gaseous states lactide synthesized and impurities formed upon synthesis in step (a); (c) liquefying gaseous components in step (b) and solidifying only lactide, to thereby separate the impurities from the thus-obtained solidified lactide; and (d) returning the separated impurities in step (c) back to the synthesis step (a). The apparatus used for the above production includes (a) a reactor for carrying out synthesis of lactide; (b) a means for gasifying synthesized lactide and impurities formed upon synthesis in the reactor (a) and discharging the resulting gaseous components; (c) a means for cooling the gaseous components to liquefy the gaseous components obtained by the means (b) and solidify only lactide; and (d) a pipe for returning to the reactor (a) components which are not solidified by the means (c).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing lactide, comprising the steps of: (a) synthesizing lactide from lactic acid; (b) gasifying the synthesized lactide and impurities formed in step (a); (c) cooling the gaseous lactide and the gaseous impurities to solidify only the gaseous lactide and to separate the solidified lactide from the impurities; (d) raising the temperature of the solidified lactide without melting the solidified lactide and to leak out the impurities from the solidified lactide; and (e) returning the impurities in step (c) back to step (a).

  2. Claim 2Depends on #1

    The method according to claim 1, wherein the synthesized lactide and impurities are heated to a temperature of from 190° to 210° C. to gasify the lactide and impurities in step (b).

  3. Claim 3Depends on #1

    The method according to claim 1, wherein the synthesized lactide and impurities