hottub.patents
US 5,779,871 A#8823344 Most CitedExpiredUnited States (USPTO)Utility

Process of manufacturing aluminum surfaces for technical lighting purposes

11Forward Citations (#8823344 Global)
0.4/yrCitation Velocity (#20739226 Global)
4.23Citation PageRank (#4343031 Global)
9Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Reflector for technical lighting purposes, having a reflecting surface of aluminum and a protective, transparent, pore-free barrier layer of aluminum oxide produced by anodizing having a dielectric constant ε of 6 to 10.5 at 20° C., where the barrier layer is of thickness d that either satisfies the condition a) for constructive interference: d·n=k·γ/2±20 nm or b) for achieving a color-toned reflector surface: k·γ/2+20 nm!<d·n< (k+1)·γ/2-20 nm! or c) for using as starting material to produce reflectors with low index/high index multi-layer coatings that increase reflectivity. d·n=l·γ/4±20 nm where n is the refractive index of the barrier layer, λ is the average wave length of the light striking the surface of the reflector, k is a natural number and l is a natural number that is uneven. The thickness of the barrier layer lies between 60 and 490 nm and does not vary by more than ±5% over the whole of the aluminum surface. The aluminum surface is anodically oxidized in an electrolyte that does not redissolve the aluminum oxide layer. The electrolyte may be a solution of organic or inorganic acids such as sulphuric or phosphoric acids at low concentrations, boric acid, adipic ac

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Process for manufacturing a reflector having a reflecting surface of aluminum and a protective, transparent, pore-free barrier layer of aluminum oxide produced by anodizing having a dielectric constant ε of 6 to 10.5 at 20° C., where the barrier layer is of thickness d that satisfies at least one of the following conditions: a) for constructive interference: d·n=k·λ/2±20 nm, b) for achieving a color-toned reflector surface: k·λ/2+20 nm!<d·n< (k+1)·λ/2-20 nm!, and c) for using as starting material to produce reflectors with low index/high index multi-layer coatings tha

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • E. Cojocaru, Analytical solutions for zero phase shift transparent coatings on metallic reflectors at 10.6 m, Applied Optics , vol. 32, No. 25, Sep. 1993.
  • E. Cojocaru, Analytical solutions for zero-phase-shift transparent coatings on metallic reflectors at 10.6 μm, Applied Optics, vol. 32, No. 25, Sep. 1993.
  • J.T. Cox et al, Aluminum mirrors Al 2 O 3 protected . . . , Applied Optics , vol. 17, No. 3, pp. 333 334, Feb. 1978.
  • J.T. Cox et al, Aluminum mirrors Al2 O3 -protected . . . , Applied Optics, vol. 17, No. 3, pp. 333-334, Feb. 1978.