Method of making exhaust valves for use in automobiles
Abstract
A method of making an exhaust valve for use in an automobile is disclosed. The exhaust valve is manufactured by forging Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy at a temperature of 1000 DEG -1200 DEG C., and annealing the forged alloy by cooling after maintaining it at a temperature of 1020 DEG -1060 DEG C. for 0.5-1.5 hours. The method further includes the step of stress relieving the forged alloy, the stress relieving step including a cooling step after maintaining the forged alloy at a temperature of 600-700 DEG C. for 1.5-2.5 hours. A strain rate of the forging step is 0.5-5/S, and the cooling of the annealing step includes a control cooling step at 0.6 DEG -0.7 DEG C./sec or the cooling of the stress relieving step includes an air cooling step. The exhaust valve has improved hardness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of making an exhaust valve, comprising the steps of: forging Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy at a temperature of 1000°-1200° C.; annealing the forged alloy by cooling after maintaining it at a temperature of 1020°-1060° C. for 0.5-1.5 hours; and comprising the further step of stress relieving the forged alloy, wherein the stress relieving step comprises the step of cooling after maintaining the forged alloy at a temperature of 600°-700° C. for 1.5-2.5 hours.
- Claim 2Depends on #1
A method according to claim 1, wherein a strain rate of the forging step is below 5/S.
- Claim 3Depends on #1
A method according to claim 1, wherein the cooling of the annealing step comprises the step of control cooling at 0.6°-0.7° C./sec.
Technical Overview & Description