US 5,778,506 A#13996221 Most CitedExpiredUnited States (USPTO)Utility

Method for ballistically enhancing a formed panel

8Forward Citations (#13996221 Global)
0.3/yrCitation Velocity (#26272765 Global)
1.36Citation PageRank (#26627443 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method to retrofit a vehicle panel with a ballistic enhancement mat sta by providing a continuous batt of fibrous material. The batt is impregnated with a matrix of material that is, or can be made to be, deformable and then hardened. The batt is cut into mats shaped in an outline of the panel. An individual mat is placed on the panel and conformed to the topography of the panel to create a surface-to-surface interface between the mat and the panel. The mat and panel are fixed together at points all over the interface via an adhesive, a hook-and-loop layer, threaded fasteners or any other suitable mechanical fastening mechanism. The matrix is then hardened, whereby the mat becomes an integral reinforcement mechanism for the panel. The matrix material can be resoftened to facilitate removal of the mat if the mat needs replacement.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of reinforcing a nonplanar panel in a vehicle or other enclosed structure both against explosive blasts and flying debris, comprising: providing a mat comprised of at least one plastically deformable matrix and fibrous material impregnated by the matrix; cutting the mat to the outline shape of the panel; placing the mat on the panel and conforming the mat to the topography of the panel, thereby creating a surface-to-surface interface between the mat and the panel; removably fixing the mat to the panel at points all over the interface; and after conforming the mat to the topogr

  2. Claim 2Depends on #1

    The method of claim 1 wherein the matrix is less malleable than the panel at ambient temperatures.

  3. Claim 3Depends on #2

    The method of claim 2 wherein at least some of the fibrous materia