Patents
US 5,777,056 A#25787004 Most CitedExpiredUnited States (USPTO)Utility

Polyolefinic resin and a resin composition comprising said resin

4Forward Citations (#25787004 Global)
0.1/yrCitation Velocity (#39471224 Global)
1.27Citation PageRank (#29592102 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A polyolefinic resin which is a homopolymer of an olefin or a copolymer of olefins, has (i) intrinsic viscosity η! measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and (ii) content of insoluble fraction in boiling n-heptane (W) in the range of 10 to 99 weight % and shows (iii) relation between relaxation time of rubber component measured by pulse NMR at the temperature of 30° C. T 2H R (30):μs!, relaxation time of rubber component measured by pulse NMR at the temperature of 80° C. T 2H R (80):μs! and the content of insoluble fraction in boiling n-heptane (W) satisfying the following equations: T.sub.2H.sup.R (80)≦670-2.2×W T.sub.2H.sup.R (80)/T.sub.2H.sup.R (30)≦8.8+0.086×W and a propylenic resin composition comprising (A) 10 to 95 weight % of the polyolefinic resin, particularly a propylenic resin which is at least one kind selected from a homopolymer of propylene and copolymers of propylene containing 4 mol % or less of other olefinic units, and (B) 90 to 5 weight % of a propylenic random copolymer having intrinsic viscosity η! measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and containing 10 to 80 m

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A polyolefinic resin which is a homopolymer or a copolymer of propylene, has (i) intrinsic viscosity η! measured in decaline at the temperature of 135° C. in the range of 0.5 to 10 deciliter/g and (ii) content of insoluble fraction in boiling n-heptane (W) in the range of 10 to 99 weight % and shows (iii) relation between relaxation time of rubber component measured by pulse NMR at the temperature of 30° C. T 2H R (30):μs!, relaxation time of rubber component measured by pulse NMR at the temperature of 80° C. T 2H R (80):μs! and the content of insoluble fraction in boiling n-heptane (

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗