Enamel frit composition for a low-expansion crystallized glass and enamel-coated low-expansion crystallized glass plate using the same
Abstract
In order to provide an enamel frit composition capable of preventing a hue of a low-expansion crystallized glass plate of a dark color from being seen through an enamel coating without increasing the thickness of the enamel coating and the mixing ratio of a coloring pigment as well as to provide an enamel-coated low-expansion crystallized glass plate using the above-mentioned composition, the enamel frit composition for a low-expansion crystallized glass essentially consists, by weight, of 30-94 wt % glass powder, 5-69 wt % TiO 2 powder, and 0.05-34 wt % coloring pigment.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An enamel-coated low-expansion crystallized glass plate comprising a low-expansion crystallized glass plate covered with an enamel coating, wherein said enamel coating consists essentially of, by weight, of about 30-94 wt % glass component, 5-69 wt % TiO 2 crystals, and 0.05-34 wt % coloring pigment component, said glass component consisting essentially of, by weight, of about 45-75% SiO 2 , 10-30% B 2 O 3 , 1-8% Al 2 O 3 , 1-10% BaO, 0-10% Na 2 O, 0-5% K 2 O, 0-5% Li 2 O, and 0-2% F 2 .
- Claim 2Depends on #1
An enamel-coated low-expansion crystallized glass plate as claimed in claim 1, wherein the content of said TiO 2 crystals is greater than that of said coloring pigment component.
- Claim 3Depends on #1
An enamel-coated low-expansion crystallized glass plate as claimed in claim 1, wherein said low-expansion crystallized glass plate consist
Technical Overview & Description