Abstract

A method for mitigating general corrosion and crack initiation and growth on the surface of a metal components in a water-cooled nuclear reactor. A compound containing a non-noble metal such as zirconium or titanium is injected into the water of the reactor in the form of a solution or suspension. This compound decomposes under reactor thermal conditions to release ions or atoms of the non-noble metal which incorporate in the surfaces of the components, including the interior surfaces of any cracks formed therein. The preferred compounds are zirconium compounds such as zirconium acetylacetonate, zirconium nitrate and zirconyl nitrate. Zirconium incorporated in the oxided surface of a metal component will reduce the electrochemical corrosion potential at the surface to a level below the critical potential to protect against intergranular stress corrosion cracking without the addition of hydrogen.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 45.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for treating a metal component to mitigate cracking in a surface of said metal component during use in a water-cooled nuclear reactor or associated equipment, comprising the steps of: forming an oxide film on said surface of said metal component; and doping said oxide film with species selected from the group consisting of a non-noble metal and a non-metal which is conductive or semi-conductive whereby said species are incorporated in said oxide film to reduce the electrochemical corrosion potential of said surface and thereby mitigate cracking.

  2. Claim 2Depends on #1

    The method as defined in claim 1, wherein said non-noble metal is selected from the group consisting of zirconium, hafnium, tantalum, niobium, yttrium, ytterbium, tungsten, vanadium, titanium, molybdenum, cerium, chromium, nickel and germanium.

  3. Claim 3Independent Claim

    The met

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 45 total)

PatentTitleYearCitations
US 6,488,782 B2Method of reducing corrosion potential and stress corrosion cracking susceptibility in nickel-based alloys20023
US 9,771,482 B2Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof20170
US 6,602,445 B2Method for the prevention of high temperatures corrosion due to alkali sulfates and chlorides using molybdenum20032
US 7,449,101 B2Method of reducing corrosion of metal material20084
US 2004258192 A1Mitigation of steam turbine stress corrosion cracking—19
US 9,969,889 B2Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof20180
US 8,320,514 B2Nuclear power plant, method of forming corrosion-resistant coating therefor, and method of operating nuclear power plant20120
US 2003029523 A1Method of reducing corrosion potential and stress corrosion cracking susceptibility in nickel-base alloys—0
US 10,006,127 B2Method for suppressing corrosion in plant and plant20180
US 6,482,528 B2Nickel-base alloy product and method of producing the same200211
US 2008137796 A1Method for reducing carbon steel corrosion in high temperature, high pressure water—9
US 6,714,618 B1Temperature-based method for controlling the amount of metal applied to metal oxide surfaces to reduce corrosion and stress corrosion cracking200413
US 9,062,878 B2Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof20150
US 2006146975 A1Nuclear power plant, method of forming corrosion-resistant coating therefor, and method of operating nuclear power plant—19
US 2004086648 A1Hydrothermal deposition of thin and adherent metal oxide coatings for high temperature corrosion protection—5