hottub.patents
US 5,773,786 A#33547449 Most CitedExpiredUnited States (USPTO)Utility

Method and device for reducing overpenetration at the start of plasma arc welds

3Forward Citations (#33547449 Global)
0.1/yrCitation Velocity (#44053907 Global)
1.03Citation PageRank (#40096809 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A shim for improving plasma arc weld quality has ends tapered at about 25° and notches at each end roughly centered over the corner between the tapered ends and main body of the shim. The improved shim allows lower starting plasma arc heat input and reduces the occurrence of sagging, or overpenetration, of the weld.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of plasma arc welding two workpieces together while reducing weld overpenetration, comprising: providing two workpieces to be welded together in close proximity to each other; providing a shim comprising a shim body having top and bottom edges, the body having a generally rectangular shape with opposite ends which taper away from the body and a pair of notches in the top edge of the shim body, one notch located over each corner formed between the bottom edge of the shim body and each tapered end, the shim positioned between the workpieces; starting a plasma arc weld keyhole adjace

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗