Dense fine grained monotungsten carbide-transition metal cemented carbide body and preparation thereof
Abstract
A cemented tungsten carbide body having a transition metal binder phase selected from the group consisting of iron, nickel and cobalt is formed, wherein the WC grains have an average WC grain size of at most about 0.5 micrometer in diameter and a maximum WC grain size of at most about 0.8 micrometer in diameter. Also, about 50 percent by volume of the WC grains in the body are angular grains and the body (1) contains an amount of the transition metal ranging from about 3 percent to about 18 percent by weight of the body, (2) is essentially free of grain growth inhibitors and (3) is essentially pore free. Said cemented tungsten carbide body is formed by mechanically mixing a source of WC with a source of transition metal, shaping the mixture into a porous body and sintering the porous body at a sintering temperature, superatmospheric pressure and time at temperature and time at superatmospheric pressure sufficient to form the cemented tungsten carbide body, wherein the sintering occurs without the formation of a liquid in the body and at least a portion of the time at superatmospheric pressure is at the sintering temperature.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 36.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A cemented carbide body comprising: (I) a transition metal binder phase, the transition metal of the transition metal binder phase being selected from the group consisting of iron, nickel, cobalt and mixture thereof, and (II) WC grains dispersed within the metal binder phase, the WC grains having an average WC grain size of at most about 0.5 micrometer in diameter wherein 99 percent by number of the WC grains have a diameter of at most about 0.8 micron and at least about 50 percent by volume of the WC grains are angular grains and the body: (1) contains an amount of the transition metal rang
- Claim 2Depends on #1
The body of claim 1 wherein the average grain size is at most about 0.3 micrometer in
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 36 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- Almond et al., "Very-Fine-Grained Hardmetals," International Journal of Refractory & Hard Metals, vol. 6, No. 3, Sep. 1987.
- Almond et al., Very Fine Grained Hardmetals, International Journal of Refractory & Hard Metals, vol. 6, No. 3, Sep. 1987.
- Bock et al., "Powder Metallurgy--Inhibition of Grain Growth on Submicron Cemented Carbides," pmi, vol. 24, No. 1, pp. 20-26 (1992).
- Bock et al., Powder Metallurgy Inhibition of Grain Growth on Submicron Cemented Carbides, pmi, vol. 24, No. 1, pp. 20 26 (1992).
- CA 2020 093, Composite hard abrasion resistant article is formed from precursor particles of metallic matrix contg. non metallic cpd. particles, Derwent 91 087629/13.