Method and apparatus for the production of polyamides
Abstract
There are proposed a method and a device for manufacturing polyamides, in which polyamide granulate manufactured by polycondensation in the molten mass is after-condensed in the solid phase, being heated. The polyamide granulate is heated in one step to a first temperature of between 70° C. and 150° C., and held for a predetermined period of time at this temperature, and then, in a second step, is heated to a second higher temperature, however lying beneath the melting point, and is after-condensed at this temperature, until the desired average degree of polycondensation is achieved.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 25.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Method of manufacturing polyamide, comprising: (a) producing a polyamide granulate by melt phase polycondensation; and (b) post-condensing said polyamide granulate in the solid state by (1) heating said polyamide granulate to a first temperature, from about 70° C. to about 150° C., and maintaining said first temperature for a predetermined period of time sufficient to decompose oligomers present with the polyamide granulate, and (2) subsequently heating said polyamide granulate to a second temperature until the desired average degree of polycondensation is achieved, said second temperature
- Claim 2Depends on #1
Method according to claim 1, wherein said predetermined period of time is from about 2 to about 6 hours.
- Claim 3Depends on #1
Method according to claim 1, wherein po
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗