Patents
US 5,773,142 A#12936964 Most CitedExpiredUnited States (USPTO)Utility

Biaxially oriented multilayered polyolefin film sealable on both sides

8Forward Citations (#12936964 Global)
0.3/yrCitation Velocity (#26010583 Global)
2.17Citation PageRank (#12734720 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A transparent, coextruded mutilayered polyolefin film which can be sealed on both sides and having a base layer essentially comprised of a resin-modified propylene polymer and top layers essentially comprised of sealable olefin polymers. At 120 DEG C., the multilayered film has a shrinkage in the longitudinal direction of more than 7% and a shrinkage in the transverse direction of more than 5%. The base layer of the film is essentially comprised of a peroxidically degraded propylene polymer, with the degradation factor A being in the range of 3 to 10, and it contains 5 to 25% of a hydrocarbon resin. The top layers of the multilayered film are essentially comprised of a random ethylene/propylene copolymer having an ethylene content of 2 to 8% by weight, a distribution factor VF of more than 8, and a thermooxidation temperature TOX of more than 230 DEG C. The film exhibits a surface gloss (angle of measurement 20 DEG ) of more than 100 and a haze (measured on four superimposed film plies) of less than 22%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A transparent, coextruded multilayered polyolefin film which can be sealed on both sides, comprising a base layer comprised of a propylene polymer, and surface layers comprised of sealable olefin polymers, wherein: a) at 120° C., the multilayered film has a shrinkage in the longitudinal direction of more than about 7%, and a shrinkage in the transverse direction of more than about 5%; b) the base layer of the multilayered film comprises a peroxidically degraded propylene polymer, having a degradation factor in the range of from about 3 to 10, and a melting point in the range of from about 16

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 3,940,379 AProcess for controlled degradation of propylene polymers197656
US 4,147,827 ACoextruded heat sealable laminar thermoplastic films1979114
EP 0,008,904 A2Heat sealable polypropylene film and method for its production—8
US 4,294,889 AResin compositions and heat-sealable composite biaxially-stretched films198137
US 4,297,415 AHeat-sealable polypropylene films198124
US 4,345,005 AOriented polypropylene film substrate and method of manufacture198245
US 4,348,457 ASealable multilayer film of polyolefins198233
US 4,384,024 AComposite heat-sealable films198343
US 4,390,385 AHeat sealable, multi-ply polypropylene film198338
US 4,419,411 AMulti-layer polypropylene film structure and method of forming same198395
US 4,439,478 AHeat sealable, multi-ply polypropylene film198433
US 4,439,493 AMultilayer heat sealable oriented packaging film and method of forming same198475
US 4,495,027 AMethod of making an oriented multilayer heat sealable packaging film198511
US 4,692,380 AMetallizable polypropylene film198757
EP 0,236,945 A2Monodispersed glycol suspension of fine inorganic oxide particles having excellent dispersion stability and method of improving the slipperiness of polyester film using the monodispersed suspension—79
US 4,734,317 ABiaxially oriented polyolefin multi-layer film198860
US 4,740,421 APolypropylene composite stretched film198816
GB 2,201,407 AAmorphous silica or silica-alumina spherical particles and process for preparation thereof—32
EP 0,340,579 A2Heat-sealable shrink film based on polypropylene, process for making it and its use for shrinkable labels—18
US 5,017,430 AHeat sealable packaging film with drawable primer199117
US 5,089,319 ABiaxially-oriented polyolefin multi-layer film which can be sealed on both sides and the preparation and use of the same199215

Non-Patent Literature (2)

  • C. Tzoganakis, et al., "Effect of Molecular Weight Distribution on the Rheological and Mechanical Properties of Polypropylene", Polymer Eng. and Science, vol. 29, No. 6, Mar. 1989, pp. 390-396.
  • C. Tzoganakis, et al., Effect of Molecular Weight Distribution on the Rheological and Mechanical Properties of Polypropylene , Polymer Eng. and Science, vol. 29, No. 6, Mar. 1989, pp. 390 396.