Composite polyester/PVA barrier films
Abstract
Polyester-based, biaxially oriented composite films having good transparency and gas-barrier properties, exhibiting excellent resistance to mechanical shock and being easily recyclable, comprise a polyester base film (for example shaped from polyethylene terephthalate) 5 μm to 50 μm in thickness, coated on at least one of its two face surfaces with a layer of polyvinyl alcohol having a number-average degree of polymerization equal to or greater than 350 and a thickness less than or equal to 0.3 μm, the mean roughness Rz of the base film being less than or equal to 0.30 μm on the at least one face surface of the film onto which a polyvinyl alcohol layer is coated and said at least one coated face surface comprising, on average, not more than 20 peaks of a height equal to or greater than 1 micrometer and not more than 150 peaks of a height ranging from 0.4 to 1 micrometer, per square millimeter, and such composite films exhibiting a permeability to oxygen, measured at 23° C. at 50% relative humidity, less than or equal to 3 cm 3 /m 2 /24 h.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for the preparation of a polyester-based, biaxially oriented composite film having good gas barrier properties, comprising: coating a polyester base film on at least one of its two face surfaces with an aqueous solution of polyvinyl alcohol which comprises at least 95% of vinyl alcohol recurring structural units, said polyvinyl alcohol exhibiting, in aqueous solution at a concentration of 4% and at 120° C., a viscosity of at least 4 mPa.s; and, heat-treating the coated film at a temperature of at least 170° C.
- Claim 2Depends on #1
The process as defined by claim 1, comprising coating a monoaxially oriented polyester base film with said aqueous PVA solution, and thereafter biaxially orienting the coated film.
- Claim 3Depends on #1
The process as defined by claim 1, said aqueous solution of polyvinyl alcohol having a concentration of 5% to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (5)
- Database WPI, Week 8712, Derwent Publications Ltd., London, GB; AN 87 082327 & JP A 62 032 048.
- Database WPI, Week 8712, Derwent Publications Ltd., London, GB; AN 87-082327 & JP-A-62 032 048.
- Database WPI, Week 8750, Derwent Publications Ltd., London, GB; AN 87 351332 & JP A 62 253 435.
- Database WPI, Week 8750, Derwent Publications Ltd., London, GB; AN 87-351332 & JP-A-62 253 435.
- Database WPI, Week 8939, Derwent Publications Ltd., London, GB; AN 89 283002 & JP A 1,208,132.