Abstract

The invention relates to the coating of flat glass with indium oxide. Indium oxide coatings, optionally doped, for example with tin, are produced in high yield by utilising a chemical vapour deposition process in which a gaseous mixture of a dialkylindium compound and a source of oxygen is directed on to the hot glass surface (The dialkylindium may also be used without pre-mixing but with separate supply of the oxygen source to the glass surface). The processes of the invention are especially suitable for application of a doped indium oxide coating to a continuous ribbon of glass on the production line on which the glass is formed, for use, for example, in architectural glazing applications utilising the low emissivity of the coating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for applying an indium oxide coating to flat glass comprises directing a dialkyl indium compound in vapour form onto a hot glass surface in the presence of a source of oxygen whereby the indium compound decomposes with formation of said indium oxide coating on the hot glass surface.

  2. Claim 2Depends on #1

    A process as claimed in claim 1, which comprises forming a mixture of the dialkylindium compound with a source of oxygen and directing the mixture in vapour form onto the hot glass surface.

  3. Claim 3Depends on #1

    A process as claimed in claim 1, wherein the indium compound is admixed with a source of oxygen before being directed onto the glass and the mixture directed over the hot glass surface under laminar flow conditions.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 33 total)

PatentTitleYearCitations
US 2006188730 A1Anti-reflective, thermally insulated glazing articles—68
US 2011023545 A1Method of producing transparent conductive film glass—16
US 2004045320 A1Method for transporting glass panels through a coating installation and device for transporting said glass panels—2
US 2010040892 A1Coated article with transparent conductive oxide film doped to adjust Fermi level, and method of making same—6
CN 111,848,695 BCatalyst and application thereof in synthesis of aromatic fluorine compound20220
US 7,482,060 B2Silicon oxycarbide coatings having durable hydrophilic properties20099
US 2008011018 A1Device for transporting glazing through a coating-depositing plant—0
US 2006248923 A1Method of making float glass with transparent conductive oxide (TCO) film integrally formed on tin bath side of glass and corresponding product—18
US 2007236618 A1Touch Screen Having Reduced Visibility Transparent Conductor Pattern—119
US 8,264,466 B2Touch screen having reduced visibility transparent conductor pattern20126
US 7,743,630 B2Method of making float glass with transparent conductive oxide (TCO) film integrally formed on tin bath side of glass and corresponding product201011
WO 2021/165680 A1Coated glass articles—0
US 7,628,896 B2Coated article with transparent conductive oxide film doped to adjust Fermi level, and method of making same20096
US 2004027339 A1Multifunctional multilayer optical film—88
US 2009155619 A1Light Transmittance Optimizing Coated Glass Article for Solar Cell and Method for Making—7

Non-Patent Literature (5)

  • Maruyama et al, J. Appl. Phys. 70(7), Oct. 1991, pp. 3848 3851.
  • Maruyama et al, J. Appl. Phys. 70(7), Oct. 1991, pp. 3848-3851.
  • Maruyama et al, J. Appl. Phys. 71(6), Mar. 1992, pp. 2915 2917.
  • Maruyama et al, J. Appl. Phys. 71(6), Mar. 1992, pp. 2915-2917.
  • Maruyama et al, Jpn. J. Appl. Phys., Part 2, 28(7), 1989, L1096 L1097.