Patents
US 5,772,800 A#17654714 Most CitedExpiredUnited States (USPTO)Utility

Aluminium alloy plate and method for its manufacture

6Forward Citations (#17654714 Global)
0.2/yrCitation Velocity (#32131330 Global)
1.64Citation PageRank (#19822768 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An aluminium alloy plate is provided with a thickness of more than 2 inches, e.g. 6, 7 or 8 inches, and having an average logarithmic fatigue life of more than 100,000 cycles determined in accordance with ASTM test method E 466. The density of micropores with a size larger than 80 μm in all locations in the midplane (T/2) midwidth position at head and tail ends of the finished plate as measured by Optical Microscopy of samples in any plane perpendicular to the midplane is less than 0.025 micropores per cm 2 . The plate may be formed by degassing of a melt to give a specified porosity of the cast ingot, and by hot rolling with at least one specified high reduction ratio pass.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An aluminium alloy plate with a thickness of more than 2 inches having an average logarithmic fatigue life of more than 100,000 cycles determined in accordance with ASTM test method E 466, wherein the density of micropores with a size larger than 80 μm in the midplane (T/2) midwidth (W/2) position at head and tail ends of the finished plate as measured by Optical Microscopy of samples in a plane perpendicular to the width direction is less than 0.025 micropores per cm 2 and the volume porosity of the plate is less than 0.005%.

  2. Claim 2Depends on #1

    A plate in accordance with claim 1 wherein the density of micropores with a size larger than 65 μm in the midplane (T/2) midwidth (W/2) position at head and tail ends of the finished plate as measured by Optical Microscopy of samples in a plane perpendicular to the width direction is less than 0.025 micro

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Advances If Fracture Research" Proc 7th Int. Conf. Houston, Texas 20-24, Mar. 1989, Pergamon, Oxford, GB, 1989 vol. 2, pp. 999-1007 P.E. Magnusen, et al The Influence of Material Quality on Airframe Structural Durability Figures 2, 3, Table 1.
  • Advances If Fracture Research Proc 7th Int. Conf. Houston, Texas 20 24, Mar. 1989, Pergamon, Oxford, GB, 1989 vol. 2, pp. 999 1007 P.E. Magnusen, et al The Influence of Material Quality on Airframe Structural Durability Figures 2, 3, Table 1.
  • Journal of Testing and Evaluation, vol. 18, nr. 1, Jan. 1990, Phil., USA pp. 439 445, Magnusen, et al Durability Assessment Based On . . . .
  • Journal of Testing and Evaluation, vol. 18, nr. 1, Jan. 1990, Phil., USA pp. 439-445, Magnusen, et al "Durability Assessment Based On . . . ".
  • Metallurgical Transactions, vol. 4, Apr. 1973, N.Y., USA, pp. 1069 1076, D H. Chien, et al Cast Microstructure and Fatigue Behavior of A High Strength Aluminium Alloy (DO 1) .