Patents
US 5,753,530 A#5001666 Most CitedExpiredUnited States (USPTO)Utility

Impurity doping method with diffusion source of boron-silicide film

18Forward Citations (#5001666 Global)
0.6/yrCitation Velocity (#12305847 Global)
2.50Citation PageRank (#10178132 Global)
25Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A solid phase diffusion process using boron silicide film as diffusion source to improve controllability of diffusion of boron impurity into a silicon substrate in order to achieve a shallow junction. The process includes: cleaning the surface of a Si substrate by removing the native oxide film thereof to expose an active surface; treating the active surface to form thereon a boron silicide film as an impurity source; and introducing boron impurity from the boron silicide film into the Si substrate to form a boron diffusion layer. In this manner, a boron diffusion layer having a high surface concentration and a shallow junction can be formed because the boron silicide film is formed directly on the surface of the Si substrate. Because the boron silicide film is chemically and physically stable, an improved diffusion controllability is obtained. The diffusion controllability is further improved by accurately evaluating the impurity film optically during the fabrication process. A structure composed of a boron diffusion layer and a boron silicide region provides a high speed, highly integrated, and highly reliable semiconductor device, particularly when the boron silicide region is d

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for fabricating a semiconductor device comprising the steps of: forming a silicon oxide layer on a silicon substrate; removing a portion of the silicon oxide layer to expose an active silicon surface; cleaning a surface of a silicon region, by procedure which includes heating a surface of the silicon region in a chamber at a temperature of 8500° C. or higher, evacuating a chamber at a background pressure of less than 5×10 -7 torr, and applying H 2 gas at a pressure of more than 1×10 -4 torr to expose an active silicon surface; forming a boron film on the exposed active

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)