US 5,750,437 A#8766349 Most CitedExpiredUnited States (USPTO)Utility

Method of fabricating semiconductor device

11Forward Citations (#8766349 Global)
0.4/yrCitation Velocity (#20729613 Global)
6.27Citation PageRank (#2290435 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a method of fabricating a semiconductor device, including the steps of (a) forming impurity-diffused layers at a surface of a silicon semiconductor substrate in selected regions, (b) forming a refractory metal film over the impurity-diffused layers, (c) carrying out first thermal annealing in nitrogen atmosphere to convert the refractory metal film into a refractory metal silicide layer, (d) causing damage to a denaturated layer having been formed over the refractory metal film due to the first thermal annealing, (e) etching both the denaturated layer and non-reacted portions of the refractory metal film with a solution containing ammonia and hydrogen peroxide therein, and (f) carrying out second thermal annealing in nitrogen atmosphere to reduce resistance of the refractory metal silicide layer. For instance, the damage is caused to the denaturated layer by arsenic (As) ion implantation. The damage may be caused to the denaturated layer by exposing to oxygen plasma. As an alternative, the damage may be caused to the denaturated layer by carrying out third thermal annealing in oxygen atmosphere at a lower temperature than a temperature at which the second thermal

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a semiconductor device, comprising the steps of: (a) forming impurity-diffused layers at a surface of a silicon semiconductor substrate in selected regions; (b) forming a refractory metal film over said impurity-diffused layers; (c) carrying out first thermal annealing to convert said refractory metal film into a refractory metal silicide layer; (d) causing damage to a denaturated layer having been formed over said refractory metal film due to said first thermal annealing; (e) etching both said denaturated layer and non-reacted portions of said refractory metal

  2. Claim 2Depends on #1

    The method as set forth in claim 1, wherein said first thermal annealing is carried out in nitrogen (N 2 ) atmosphere in

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗