Abstract

A melt-extrudable thermoplastic polypropylene composition having a melt flow rate in a range of from about 18 to about 30 g/10 minutes at a temperature of 190 DEG C. and a load of 2.16 kg, a polydispersity less than 4, and a Z-average molecular weight greater than 300,000 as determined by differential refractometry. The composition may include a first thermoplastic polypropylene having a melt flow rate lower than 18 g/10 minutes at a temperature of 190 DEG C. and a load of 2.16 kg and a second thermoplastic polypropylene having a melt flow rate higher than 18 g/10 minutes at a temperature of 190 DEG C. and a load of 2.16 kg. The weight ratio of the first polypropylene to the second polypropylene is in a range of from about 90:10 to about 10:90. The composition may include from about 0.1 to about 1 percent by weight, based on the weight of the first and second thermoplastic polypropylenes, of a defined alkyl-substituted polysiloxane. A method of forming a nonwoven web also is provided, which method involves compounding the melt-extrudable thermoplastic polypropylene composition composed of a first and second thermoplastic polypropylene as described above. The compounded thermoplasti

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 22.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A composition comprising a melt-extrudable thermoplastic polypropylene composition having: a melt flow rate in a range of from about 18 to about 30 g/10 minutes at a temperature of 190° C. and a load of 2.16 kg; a polydispersity less than 4; and a Z-average molecular weight greater than 300,000 as determined by differential refractometry.

  2. Claim 2Depends on #1

    The composition of claim 1 which further comprises from about 0.1 to about 1 percent by weight, based on the weight of the thermoplastic polypropylene, of an alkyl-substituted polysiloxane having the general formula, ##STR4## in which: R 1 -R 9 are independently selected monovalent C 1 -C 3 alkyl groups; R 10 is a monovalent C 6 -C 30 alkyl group; m represents an integer of from about 5 to about 50; n represents an integer of from 0 to about 200; the alkyl-substituted polysil