Polypropylene resin composition for exterior parts of automobile
Abstract
A polypropylene resin composition having a high moldability and capable of forming therefrom shaped articles having excellent surface hardness, thermal deformation resistance and low temperature impact resistance includes (A) 35-74 wt % of a crystalline ethylene-propylene block copolymer with an ethylene content of 0.5-15 wt %, an isotactic pentad fractional propylene of 96% or more and a MFR of 40-80 g/10 min. (230 DEG C., 2160 g); (B) 21-40 wt % of an ethylene- alpha -olefin copolymer produced by using a single site catalyst and having an alpha -olefin content of 70 mol % or more, a ratio (Mw/Mn) of 2.5 or less, and a ratio (MI10/MI2.16) of 6 to 15; and (C) 5-25 wt % of a talc particle component having an average particle size of 3-7 mu m.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 18.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A polypropylene resin composition for the exterior parts of automobiles, comprising: (A) 35 to 74% by weight of a crystalline ethylene-propylene block copolymer having a content of copolymerized ethylene of 0.5 to 15% by weight, an isotactic pentad fraction (mmmm) of copolymerized propylene of 96% or more, and a melt flow rate of 40 to 80 g/10 minutes determined at a temperature of 230° C. under a load of 2160 g; (B) 21 to 40% by weight of an ethylene-α-olefin copolymer prepared by a catalytic polymerization in the presence of a single site catalyst, containing 70 molar % or less of copolyme
Technical Overview & Description