Patents
US 5,741,580 A#7891801 Most CitedExpiredUnited States (USPTO)Utility

Crystalline thin film and producing method thereof, and acoustooptic deflection element

12Forward Citations (#7891801 Global)
0.4/yrCitation Velocity (#18567920 Global)
14.36Citation PageRank (#581401 Global)
0Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A thin film having a good orientation and crystallinity. A method of producing the thin film on a substrate, wherein materials of a thin film are deposited and/or crystallized on a substrate. When a laser ablation method is adopted, the temperature of the glass substrate is set in the range between 200° C. and 700° C., and the pressure of O 2 gas in a film forming chamber is set in the range between 7×10 -5 Torr and 1×10 -2 Torr. A laser beam irradiates a ZnO target. The target radiates materials of a thin film, such as neutral ions, molecules and ions, and the radiated materials are deposited and/or crystallized on the glass substrate to turn into a ZnO thin film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A preparation method of a crystalline ZnO thin film formed on a glass member comprising: irradiating a ZnO target with a laser beam in an atmospheric pressure of O 2 gas in the range between 7×10 -5 Torr and 1×10 -2 Torr; and depositing a material generated by the irradiation on a glass member heated to a temperature in the range between 200° C. and 700° C.

  2. Claim 2Depends on #1

    A method as claimed in claim 1, wherein: said atmospheric pressure of O 2 gas is in the range between 2×10 -4 Torr to 2.5×10 -3 a Torr; and said glass member is heated to a temperature in the range between 360° C. and 600° C.

  3. Claim 3Depends on #1

    A method as claimed in claim 1, wherein: said atmospheric pressure of O 2 gas is in the range between 2×10 -4 Torr to 6×10 -4 Torr; and said glass member is heated to a temperature in the range between 500° C. an

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (5)

  • C.R. AITA et al., "The Effect of O2 on reactively sputtered zinc oxide," J. Appl. Phys. 51(10), Oct. 1980, pp. 5533-5536.
  • C.R. AITA et al., The Effect of O 2 on reactively sputtered zinc oxide, J. Appl. Phys. 51(10), Oct. 1980, pp. 5533 5536.
  • Hirotoshi SATO et al., "Highly transparent and conductive group IV impurity-doped ZnO thin films prepared by radio frequency magnetron sputtering," J. Vac. Sci. Technol. A. 11,(6), Nov./Dec. 1993, pp. 2975-2979.
  • Hirotoshi SATO et al., Highly transparent and conductive group IV impurity doped ZnO thin films prepared by radio frequency magnetron sputtering, J. Vac. Sci. Technol. A. 11,(6), Nov./Dec. 1993, pp. 2975 2979.
  • Takashi Yamamoto et al., "Characterization of ZnO piezoelectric films prepared by rf planar-magnetron sputtering," J. Appl. Phys. 51(6), Jun. 1980, pp. 3113-3120.