Solutions of intermediate molecular weight polymers from about 200,000 to about 4,000,000, such as polyethylene, in a relatively non-volatile solvent are extruded through an aperature at constant concentration and thereafter stretched at a ratio of at least about 3:1 prior to cooling to form a first gel. The first gels are extracted with a volatile solvent to form a second gel, and the second gel is dried to form a low porosity xerogel. Stretching occurs with any one or more of the first gel, second gel or xerogel. The polyethylene products produced by our process include products having a molecular weight between about 200,000 and about 4,000,000 a tenacity of at least about 13 grams/denier, a modulus of at least about 350 gram/denier, a porosity of less than 10% by volume, a crystalline orientation function of at least about 0.95, and a main melting temperature of at least about 140° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 95.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A film or fiber consisting essentially of polyethylene having a weight average molecular weight between about 200,000 and less than 800,000 kg/kg mole, said fiber or film having a tensile modulus of at least 350 grams/denier, a tenacity of at least 13 grams/denier, a crystalline orientation function of at least 0.95, a main melting temperature of at least 140° C. (measured at 10° C./minute heating rate by differential scanning calorimetry), an ultimate elongation of not more than 5%, and a traverse microfibrillar spacing of less than 150 Å.

  2. Claim 2Depends on #1

    The fiber or film of claim 1 wherein the polyethylene has a weight average molecular weight between 250,000 and 750,000, and the fiber or film has a tensile modulus of at least 500 grams/denier and a tenacity of at least 15 grams/denier.

  3. Claim 3Depends on #2

    The fiber or film of claim 2 wherein the f