Patents
US 5,698,341 A#953314 Most CitedExpiredUnited States (USPTO)Utility

Carbon material for lithium secondary battery and process for producing the same

49Forward Citations (#953314 Global)
1.7/yrCitation Velocity (#2816961 Global)
34.59Citation PageRank (#132819 Global)
10Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A carbon material for use in a lithium secondary battery, which is obtained by graphitization conducted in the presence of a boric compound so as to contain boron in an amount ranging from 1,000 ppm to 30,000 ppm and which, when subjected to X-ray diffractometry, exhibits an interplanar spacing of 002 surface (d 002 ) of not greater than 0.338 nm, a crystallite size along c-axis (Lc) of at least 35 nm, a crystallite size along a-axis (La) of at least 50 nm and a ratio of diffraction peak (101) to diffraction peak (100), designated as P 101 /P 100 , of at least 1.0; a negative electrode and a lithium secondary battery each produced by using the above carbon material; and a process for producing the carbon material. This carbon material exhibits large charge and discharge capacities, so that it can provide a negative electrode for use in a lithium secondary battery which is excellent in charge and discharge cycle characteristics.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 49.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a carbon material for use in a lithium secondary battery, which comprises the steps of: spinning a mesophase pitch to thereby obtain pitch fibers; infusibilizing the pitch fibers to thereby obtain infusibilized pitch fibers; milling the thus infusibilized pitch fibers, and graphitizing the milled fibers at a temperature of not lower than 2,200° C. in the presence of a boric compound.

  2. Claim 2Independent Claim

    A process for producing a carbon material for use in a lithium secondary battery, which comprises the steps of: spinning a mesophase pitch to thereby obtain pitch fibers; infusibilizing the pitch fibers to thereby obtain infusibilized pitch fibers; subjecting said infusibilized pitch fibers to light carbonization at a temperature of not higher than 1,500° C., milling the thus lightly carbonized pitch fibers, and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Database WPI, Derwent Publications, AN 91 365343, JP A 03 245 458, Nov. 1, 1991.
  • Database WPI, Derwent Publications, AN 95 188589, JP A 07 105 955, Apr. 21, 1995.
  • Database WPI, Derwent Publications, AN-91-365343, JP-A-03 245 458, Nov. 1, 1991.
  • Database WPI, Derwent Publications, AN-95-188589, JP-A-07 105 955, Apr. 21, 1995.
  • Patent Abstracts of Japan, JP A 2 145814, Jun. 5, 1990.