Patents
US 5,698,145 A#17219097 Most CitedExpiredUnited States (USPTO)Utility

Method for producing Mn-Zn ferrites

6Forward Citations (#17219097 Global)
0.2/yrCitation Velocity (#32086989 Global)
1.80Citation PageRank (#17110321 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for sintering Mn--Zn ferrite green compacts is provided which includes a first heating step of raising the temperature from room temperature to 600° C. within a period from 30 minutes to 5 hours, a second heating step of raising the temperature from 600° C. to the sintering temperature and holding the sintering temperature until the start of cooling within a period shorter than 10 hours, and a cooling step of lowering the temperature to 150° C. within a period longer than 3 hours, with the total period of the three steps being shorter than 20 hours. This method permits the efficient production in a short time of Mn--Zn ferrites having good magnetic properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of sintering a Mn--Zn ferrite green compact in a roller hearth continuous sintering furnace comprising: a) preparing a calcined mixture of Fe 2 O 3 , MnO and ZnO, b) combining said calcined mixture with a binder consisting essentially of polyvinyl alcohol to form a metal oxide/binder mixture, c) compacting said metal oxide/binder mixture to form said Mn--Zn ferrite green compact, d) removing said binder from said compact by reaction with atmospheric gas while preheating said compact by raising the temperature from room temperature to 600° C. within a period from 30 minutes to 5

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • "Fast Sintering of Soft Mn-Zn and Ni-Zn Ferrite Pot Cores", Antoinette Morell et al, American Ceramic Society Bulletin, vol. 59, No. 6, 1980, Columbus, Ohio, pp. 62662-62629.
  • Fast Sintering of Soft Mn Zn and Ni Zn Ferrite Pot Cores , Antoinette Morell et al, American Ceramic Society Bulletin, vol. 59, No. 6, 1980, Columbus, Ohio, pp. 62662 62629.
  • Soft Ferrites by Sadataro Hiraga, Bulletin of the Japan Institute of Metals, vol. 24, No. 4 (1985) p. 288 (partial translation and copy of the Japanese reference indicating the translated part).
  • Soft Ferrites Sadatoro Hiraga, Bulletin of the Japan Institute of Metals, vol. 24, No. 4 (1985) (Partial Translation).