Patents
US 5,697,998 A#2899805 Most CitedExpiredUnited States (USPTO)Utility

Sapphire window laser edge annealing

26Forward Citations (#2899805 Global)
0.9/yrCitation Velocity (#7929179 Global)
2.98Citation PageRank (#7670987 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A sapphire window is laser edge annealed using a CO 2 laser spot illuminating along a path following the edge of the window so as to heat the edges to remove or reduce sub surface defects which can cause stress fractures.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 26.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of treating an optical ceramic having an edge and an optical surface, said edge having microscopic flaws, said optical surface is exposed to stresses during use, the method comprising the steps of, preheating said optical ceramic to a temperature below an annealing temperature of said optical ceramic, generating an illumination beam having a wavelength that can be absorbed by said optical ceramic, and illuminating said edge of said optical ceramic to heat said edge above said annealing temperature to reduce said microscopic flaws and increase edge mechanical strength while not ill

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 26 total)

PatentTitleYearCitations
WO 03,082,761 A1Reduction of damage initiation density in fused silica optics via uv laser conditioning—0
US 11,565,350 B2System and method for laser beveling and/or polishing20230
US 9,461,357 B2Antenna on sapphire structure20160
US 6,845,635 B2Method of manufacturing glass substrate for information recording media, glass substrate for information recording media manufactured using the method, and information recording medium using the glass substrate200520
US 2008037014 A1Method for reducing diameter of bubble existing in a glass plate—4
US 6,705,125 B2Reduction of damage initiation density in fused silica optics via UV laser conditioning200415
US 9,956,646 B2Multiple-beam laser processing using multiple laser beams with distinct wavelengths and/or pulse durations20182
US 10,126,061 B1Localized strengthening of features for a sapphire component20181
US 11,819,949 B2Multi-laser system and method for cutting and post-cut processing hard dielectric materials20230
US 9,764,427 B2Multi-laser system and method for cutting and post-cut processing hard dielectric materials20175
US 10,343,237 B2System and method for laser beveling and/or polishing20197
US 2002108400 A1Method of manufacturing glass substrate for information recording media, glass substrate for information recording media manufactured using the method, and information recording medium using the glass substrate—35
US 8,225,627 B2Method for reducing diameter of bubble existing in a glass plate20122
US 10,286,487 B2Laser system and method for processing sapphire20195
US 10,427,968 B2Method for cutting glass20193

Non-Patent Literature (5)

  • "CRC Handbook of Chemistry and Physics",R.C. Weast, CRC Press, Inc., 67th ed., pp. B-68, B-103, B-126, B-127, B-143, B-145, 1986-1987.
  • "CW Laser Annealing of Ion Implanted Oxidized Silicon Layers on Sapphire", by G. Alestig, et al. Mat.Res.Soc.Symp.Proc., vol. 13, 1983.
  • "Fracture in Ceramic Materials, The Thermal Fracture of Alumina", edited by A.G. Evans, et al.. pp. 336-364, 1984.
  • "High Intensity Luminescence From pulsed Laser Annealed Europium Implated Sapphire", by N. Can, et al. Appl. Phys. Lett. vol. 65, No. 15, Oct. 10, 1994.
  • "High Performance Sapphire Windows",S.C. Bates, NTIS, Technology 2002, vol. 2, pp. 460-469, Dec. 1962.